AL undertakes Chemical Testing, Mechanical Testing. The following sample requirements will provide optimal sample size for our engineers to conduct the required tests. Your sample size meet the requirements listed below, Sample sizes larger than those listed will not present a problem, the table below is considered as a good reference point for most samples.

TYPE OF TESTING

SHEET

PLATE

ANGLE

BAR

PIPE /TUBING

Chemical

50x25

50 x 50

50 Long

50 Long

50 Long

Tensile

50 W x 300 L

50 W x 300 L

300 long

350 Long

350 Long

Bend

50 W x 300 L

50 W x 300 L

-

350 Long

400 Long

Hardness

50 x 50

50 x 50

50 x 50

50 Long

50  Long

Flattening

-

-

-

-

100 Full Ring

Flaring

-

-

-

-

150 Full Ring

Wet Chemical Analysis
Metals Chips - 5 grams minimum, 10 grams preferred.
Time for Completion: 2 Days.

TMT Bar
>> 1 .2 Meter Long, Each Diameter having 3 Samples.
>> Test Conduct: Chemical Analysis, Tensile (Yield Stress, UTS, Elongation, Bend, & Rebend Test).
>> Time for Completion: 1 Day.

Weld Procedure Qualification:

>> The welded test plate should be a minimum of 300 mm Wide by 500 mm along the weld.
>> Test Conduct:
>> Time for completion – Min. 5 Days.

Note:
1. All Dimensions are in mm.
2. Grain direction is very important when submitting Plate or sheet for testing. Always mark direction with an arrow on the Sample/s.
 
 